MATERIAL OF LINING
FUSED SILICA TBF-100 EX JAPAN
September 18, 2014
– Specification      : Al2O3 = 0.40% B2O3 = 0. 00% SiO2 = 99.20% Fe2O3 = 0.30% max – Temperature : 1600° C – Usage
FUSED SILICA TBF-101 EX JAPAN
September 18, 2014
– Specification      : Al2O3 = 0.10% B2O3 =  1. 00% SiO2 = 98.50% Fe2O3 = 0.10% max – Temperature : 1600° C – Usage
FUSED SILICA TBF-102-07 EX JAPAN
September 18, 2014
– Specification      : B2O3 = 0. 70% SiO2 = 99 <% Fe2O3  = 0.10% max – Temperature : 1600° C – Usage : Melting
FUSED SILICA TBF-104 EX JAPAN
September 18, 2014
– Specification      : Al2O3 = 0.10% B2O3 = 0. 00% SiO2 = 99.50% Fe2O3 = 0.10% max – Temperature  : 1600°C – Usage :
FUSED SILICA TBF-104P EX JAPAN
September 18, 2014
– Specification      : Al2O3 = 0.10% B2O3  = 1. 00% SiO2 = 98.50% Fe2O3 = 0.10% max – Temperature : 1600° C – Usage